Price:
Melting Point : 1350C 1390C
Hardness : High, Other
Color : Silver
Grade : UNS N05500
Thickness : Varies based on requirement
Thermal Conductivity : 21 W/mK at 20C
Melting Point : 1300C
Hardness : Other, RB 6580
Color : Silver
Grade : Monel 400
Thickness : Customizable
Thermal Conductivity : 21.8 W/mK
Melting Point : 13501390 C
Hardness : Other, Approximately 3240 HRC
Color : Metallic Silver
Grade : K500
Thickness : Customizable per requirements
Thermal Conductivity : 21 W/mK
Melting Point : 13501390C
Hardness : Other, Typically 65 Rockwell B (HRB)
Color : Silver
Grade : UNS N04400
Thickness : Customizable
Thermal Conductivity : 21 W/mK